Comparison of SA-210C Boiler Tube and 20G Boiler Tube.
SA-210C (25MnG) is ASME SA-210 standard steel, is a boiler and superheater with carbon-manganese steel small-caliber tube, pearlitic heat-resistant steel.

Comparison of chemical properties of SA-210C and 20G
| Grade | Chemical Composition(%) | ||||
| C | Mn | Si | P | S | |
| ASME SA210 C | ≤0.35 | 0.29-1.06 | ≥0.10 | ≤0.035 | ≤0.035 |
| Grade | Chemical Composition(%) | |||||||||
| C | Si | Mn | P | S | Cr | Mo | Cu | Ni | V | |
| 20G | 0.17-0.24 | 0.17-0.37 | 0.70-1.00 | ≤0.03 | ≤0.03 | ≤0.25 | ≤0.15 | ≤0.2 | ≤0.25 | ≤0.08 |
| Grade | Mechanical property | ||
| Tensile Strength(MPa) | Yield Strength(MPa) | Elongation(%) | |
| ASME SA210 C | ≥485 | ≥275 | ≥30 |
20G high pressure boiler tube Mechanical property
| Grade | Mechanical property | ||
| Tensile Strength(MPa) | Yield Strength(MPa) | Elongation(%) | |
| 20G | ≥240 | ≥415 | ≥22 |
SA-210C boiler tube chemical composition is simple, in addition to carbon, manganese content is high, the rest and 20G close.
SA210C / ASTM A213 Grade C
Tubing Specifications
| SA210C / ASTM A210 Grade C Chemical Composition |
|
|---|---|
| Carbon Max: 0.35% | Silicon Min: 0.10% |
| Manganese*: 0.29-1.06% | Nickle: N/A |
| Phosphorus Max: 0.035% | Chromium: N/A |
| Sulfur Max: 0.035% | Molybdenum: N/A |
| SA210C / ASTM A210 Grade C Mechanical Properties |
|
|---|---|
| Tensile Strength | ksi: 70 MPa: 485 |
| Yield | ksi: 40 MPa: 275 |
| Maximum Hardness | |
| Rockwell B | 89 HRB Max. |
| Brinell | 179 HB Max. |
*Manganese can increase above 1.06% up to 1.35% at a rate of 0.06 for every 0.01% the carbon is below the maximum (0.35%). Elongation in 2in. or 50mm, min: 30% SA210C is a P1 Material.